Head to head

Kirschbaum P2 17L (1.20) vs Mantis Power Poly 17

P2 17L (1.20) leads on 3 of 6 measurements. The widest gap is ball bite, where P2 17L (1.20) is 16 percentile points ahead. Every figure is a testing-machine result at a fixed reference tension.

Measured, side by side

Kirschbaum

P2 17L (1.20)

Polyester · 17L ga

Mantis

Power Poly 17

Polyester · 17 ga

Stiffness lower = softer, kinder on the arm
19765th pct
20471st pct
Tension loss lower = stays where you strung it
4270th pct
4372nd pct
Energy return higher = livelier, more free power
8522nd pct
8625th pct
Spin potential higher = more spin off the string bed
4.851st pct
4.851st pct
Ball bite higher = grabs the ball harder
0.44150th pct
0.41735th pct
String friction lower = strings slide and snap back
0.09250th pct
0.08637th pct

Bars are percentile against all 791 strings, and the marked side is the one that measures better, which is not always the one you want. A firmer bed is worse for your elbow and better for your control, and no measurement knows which of those you came for.

Which one wins, by problem

Each string's standing on the site's rankings, out of every measured string in the database. This is where a comparison stops being arithmetic and starts being a decision.

Swapping between them: what tension?

Bed stiffness is published at one reference tension, so the only honest conversion is to scale it. These are starting points from 52 lb, not prescriptions. The calculator takes your own tension.

Coming from P2 17L (1.20) at 52 lb

String Power Poly 17 at 48.8 lb 22.1 kg

Coming from Power Poly 17 at 52 lb

String P2 17L (1.20) at 55.0 lb 24.9 kg

Hybrid: what if you used both?

Estimated, not measured. No hybrid combination has been tested as a bed. These figures are the two strings' own lab measurements weighted by how much of the bed each one actually is. Treat them as a guide to which way a pairing moves, never as lab data.

P2 17L (1.20) mains / Power Poly 17 crosses

Stiffness68th pct · 1 measured
Tension loss71st pct · 1 measured
Energy return23rd pct · 1 measured
Spin potential51st pct · 1 measured
Ball bite49th pct · 1 measured
String friction48th pct · 1 measured

Power Poly 17 mains / P2 17L (1.20) crosses

Stiffness69th pct · 1 measured
Tension loss71st pct · 1 measured
Energy return24th pct · 1 measured
Spin potential51st pct · 1 measured
Ball bite38th pct · 1 measured
String friction41st pct · 1 measured

Open this in the hybrid builder

Which goes dead first?

Estimated from tension loss, which is the only thing the database measures about ageing. This is when the bed stops playing the way you strung it, not when the string breaks.

P2 17L (1.20)

~19 hours of play

Power Poly 17

~18 hours of play

Both strings in full

Every published measurement
StringGaugePriceStiff lb/inLoss %Power %SpinBite COFFriction COF
Kirschbaum P2 17L (1.20) Polyester17Lfind19742854.80.4410.092
Mantis Power Poly 17 Polyester17find20443864.80.4170.086

Add a third string P2 17L (1.20) in full Power Poly 17 in full